Nanoindentation and birefringence measurements on fused silica specimen exposed to low-energy femtosecond pulses

Yves Bellouard*, Tristan Colomb, Christian Depeursinge, Mark Dugan, Ali A. Said, Philippe Bado

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

84 Scopus citations